ASC BRICK FOR IRON LADLE

WHO WE ARE :

We not only provide the best service to World Top 500 Enterprises , also to YOU .

We can accept the Payment Term : LC 120 DAYS , D/P 90 DAYS, D/A-O/A 60 DAYS .

We have more 100 items Chinese National Patents .

Our Lab is Hennan province Refractory Engineering T&R Center

Our Tech Team include : PROFESSOR , DOCTORAL SUPERVISOR , SENIOR ENGINEER, EXPERT.

Our Project Team have rich experience for international Refractory Turn-Key Project .

We are not only to supply refractory products to YOU , We also want to share the KEY TECH with YOU.

Technical instructions

ASC BRICK & CASTABLE FOR THE IRON LADLE

LIFE > 1200 HEATS .

 

It is mainly raw material made of electro-corundum (or sintered corundum, special glass bauxite clinker) and graphite and silicon carbide containing more than 90%-95% of fixed carbon.Add graphite, bauxite and additives, and make them by mixing, moulding, drying and firing at high temperature.

Technical Parameters

1、铝碳化硅碳砖 – ASC BRICK

项     目 ITEM

单位

指标值

体积密度 BD

g/cm3

 ≥2.85

常温耐压强度   CCS       

Mpa

≥40

高温抗折强度(1400℃×0.5h)MOR

Mpa

≥5

 Al2O3

%

55-65

C

%

5-12

SiC

%

8-10

2、铝碳化硅浇注料 – ASC CASTABLE (REPAIR CASTABLE )

项    目 ITEM

单位

指标值

Al2O3     

%

55-65

SiC

%

6-10

耐火度 REFRACTORINESS

>1790    

体积密度 BD

g/cm3

 ≥2.6

抗折强度

MOR

110℃×24h

Mpa

≥6

1500℃×3h

Mpa

≥10

耐压强度

CCS

110℃×24h

Mpa

≥50

1500℃×3h

Mpa

≥80

烧后线变化 PLC

1500℃×3h

%

±1

Get In Touch
Send on email.all fields width on * are required. Please enter your question and contact information.we will get back to you as soon as possible!.

    Name
    * Phone
    * E-mail
    Country

    *Your Messages

    15515811693 Whatsapp wxesxxx@126.com Message